Carbide Inserts for Turning Stainless Steel

Carbide Inserts for Turning Stainless Steel by APT Carbide

Grade M250 and Chip Breaker MPN for positive inserts and MMN for negative inserts are designed to cut all grades of stainless steel they will also cut hi-temp alloys and hi-alloy steel

Grade M250 is our most advanced Multi-PVD coated grade for machining stainless it incorporates layers of TiN and TiAlN providing excellent wear resistance with good metal removal rates but will also cope with lower cutting speeds and work hardening materials 

Grades 2235, 2230 and Chip Breakers MM and FX will be replaced with the newer models as stock is depleted, Grade 2235 is coated using the MT-CVD coating process with layers of TiN-TiCN-AlO2-TiN it produces a wear resistance coating which has the ability to cope with lower cutting speed than other CVD coatings. Grade 2230 is more wear resistant that 2235 and can cope with higher cutting speeds.

Page 3 of 5:    144 Items

1   2   3   4   5
Show All Products
1   2   3   4   5
Show All Products

Page 3 of 5:    144 Items
Recommended Cutting Conditions - Speeds and Feeds for APT Carbide Turning Inserts for Stainless Steel
Material
Chip Groove + Grade (ISO)
Cutting Speed m/min
Feed mm/rev
Depth of Cut
High Alloyed & Tool Steel 200-350 HB
MMN M250 (P30-P40)
60-140 0.20-0.40
1.0-3.5
High Alloyed & Tool Steel 200-350 HB
MPN M250 (P30-P40)
60-140
0.12-0.25
1.0-3.0
Corrosion Resistant Steel 200-325 HB
MMN M250 (P30-P40)
100-170
0.20-0.40
1.0-3.5
Corrosion Resistant Steel 200-325 HB
MPN M250 (P30-P40)
100-170
0.12-0.25
1.0-3.0
Stainless Steel 180-200 HB
MMN M250 (M30-M40)
120-190
0.20-0.40
1.0-3.5
Stainless Steel 180-200 HB
MPN M250 (M30-M40)
120-190
0.12-0.25
1.0-3.0
Duplex Stainless 230-260 HB
MMN M250 (M30-M40)
80-150
0.20-0.40
1.0-3.5
Duplex Stainless 230-260 HB
MPN M250 (M30-M40)
80-150
0.12-0.25
1.0-3.0
Hardened Stainless 330 HB
MMN M250 (M30-M40)
55-75
0.20-0.30
1.0-3.0
Hardened Stainless 330 HB
MPN M250 (M30-M40)
55-75
0.12-0.20
1.0-2.0
Iron Based Hi-temp Alloys
MMN M250 (S15-S25)
15-35
0.20-0.30
1.0-2.0
Iron Based Hi-temp Alloys
MPN M250 (S15-S25)
15-35
0.12-0.20
1.0-1.5
Nickel Based Hi-temp Alloys MMN M250 (S15-S25)
4-20
0.2-0.25
1.0-2.0
Nickel Based Hi-temp Alloys
MPN M250 (S15-S25)
4-20
0.12-0.15
1.0-1.5
Pure Titanium
MMN M250 (S15-S25)
80-130
0.20-0.30
1.0-3.0
Pure Titanium
MPN M250 (S15-S25)
80-130
0.12-0.20
1.0-2.0
Titanium  Alpha + Beta Alloys
MMN M250 (S15-S25)
15-35
0.20-0.25
1.0-2.0
Titanium  Alpha + Beta Alloys
MPN M250 (S15-S25)
15-35
0.12-0.15
1.0-1.5